Fenómeno del problema
Snakeskin-like irregular texture on the surface of EAA extruded products
Análisis de la causa
Extrusion temperature too low, uneven melt elastic recovery; uneven die temperature distribution
Solución
1) Increase extrusion temperature to the processing temperature range; 2) Homogenize die temperature to ±2°C; 3) Reduce extrusion rate to reduce elastic recovery
Conclusión clave
Snakeskin texture is caused by low-temperature extrusion and elastic recovery; raising temperature and reducing speed is key