Extrusion & Post
8 views
EAA surface snakeskin texture
Problem Phenomenon
Snakeskin-like irregular texture on the surface of EAA extruded products
Cause Analysis
Extrusion temperature too low, uneven melt elastic recovery; uneven die temperature distribution
Solution
1) Increase extrusion temperature to the processing temperature range; 2) Homogenize die temperature to ±2°C; 3) Reduce extrusion rate to reduce elastic recovery
Key Takeaway
Snakeskin texture is caused by low-temperature extrusion and elastic recovery; raising temperature and reducing speed is key
Was this helpful?
0 people found this helpful
Thank you for your feedback!