Material Drying 3 Aufrufe

Bubbles in EVA injection molded thick walls

Problembeschreibung
Dense bubbles 0.1-0.5mm appear inside EVA injection molded thick wall products, concentrated at wall thickness center
Ursachenanalyse
Holding pressure insufficient <40MPa or holding pressure time short with thick wall center not compacted; raw material contains moisture; injection speed too fast entrapping air; poor mold venting
Lösung
1) Increase holding pressure to 60-80MPa; 2) Extend holding pressure time to fully compact thick walls; 3) Fully dry raw material to moisture <0.02%; 4) Add vent grooves or vent pins to mold; 5) Progressively decelerate injection to avoid air entrapment
Wichtigste Erkenntnis
Thick wall bubbles are caused by insufficient holding pressure, moisture and poor venting combined
EVA injection bubbles holding pressure thick wall products mold venting