Material Drying 7 visualizações

Bubbles in EVA injection molded thick walls

Fenómeno do problema
Dense bubbles 0.1-0.5mm appear inside EVA injection molded thick wall products, concentrated at wall thickness center
Análise das causas
Holding pressure insufficient <40MPa or holding pressure time short with thick wall center not compacted; raw material contains moisture; injection speed too fast entrapping air; poor mold venting
Solução
1) Increase holding pressure to 60-80MPa; 2) Extend holding pressure time to fully compact thick walls; 3) Fully dry raw material to moisture <0.02%; 4) Add vent grooves or vent pins to mold; 5) Progressively decelerate injection to avoid air entrapment
Conclusão principal
Thick wall bubbles are caused by insufficient holding pressure, moisture and poor venting combined
EVA injection bubbles holding pressure thick wall products mold venting