EVA surface gloss is poor
Problembeschreibung
EVA product surface gloss <60%, below the 80% requirement, with dull appearance
Ursachenanalyse
Rough mold surface Ra>0.4μm; high EVA crystallinity with surface microcrystals scattering light; improper cooling rate
Lösung
1) Polish the mold to Ra<0.1μm mirror finish; 2) Increase mold temperature to delay crystallization and reduce scattering; 3) Add nucleating agent to control crystal size
Wichtigste Erkenntnis
Poor gloss is caused by rough mold and crystalline scattering; polishing the mold and controlling crystallization are key