Injection Molding
4 Aufrufe
EVOH Surface Orange Peel
Problembeschreibung
EVOH product surfaces show orange-peel-like uneven texture, rough to the touch
Ursachenanalyse
Mold temperature too low <30°C, product surface rapidly cools and solidifies then the interior continues to shrink causing surface unevenness; injection speed too low
Lösung
1) Increase mold temperature to 40-50°C to delay surface solidification; 2) Appropriately increase injection speed; 3) Increase holding pressure to reduce internal shrinkage
Wichtigste Erkenntnis
Orange peel is caused by rapid cooling and solidification; increasing mold temperature and holding pressure are key
War das hilfreich?
0 Personen fanden dies hilfreich