Injection Molding 1 visualizações

EVOH Surface Orange Peel

Fenómeno do problema
EVOH product surfaces show orange-peel-like uneven texture, rough to the touch
Análise das causas
Mold temperature too low <30°C, product surface rapidly cools and solidifies then the interior continues to shrink causing surface unevenness; injection speed too low
Solução
1) Increase mold temperature to 40-50°C to delay surface solidification; 2) Appropriately increase injection speed; 3) Increase holding pressure to reduce internal shrinkage
Conclusão principal
Orange peel is caused by rapid cooling and solidification; increasing mold temperature and holding pressure are key
EVOHorange peelmold temperatureholding pressuresurface solidification