DSTDP extruded film longitudinal streaks
Problembeschreibung
DSTDP extruded film surface has continuous streaks 1-3mm wide along the extrusion direction
Ursachenanalyse
Die lip locally damaged or gap uneven; unstable flow produced in the melt residence zone inside the die; pressure fluctuation at the screw front end
Lösung
1) Check die lip flatness and gap uniformity ±0.01mm; 2) clean die interior to remove carbonized matter in residence zones; 3) install gear pump on extruder to stabilize melt pressure; 4) polish die lip to Ra<0.1μm
Wichtigste Erkenntnis
Longitudinal streaks are caused by die defects and pressure fluctuation; die maintenance and pressure stability are key