Material Analysis 3 Aufrufe

DSTDP hardness too high

Problembeschreibung
DSTDP product Shore hardness 5-10 degrees higher than target, hard hand feel
Ursachenanalyse
DSTDP crystallinity on the high side, rigidity increased; filler added too much; cooling too fast, crystallization incomplete but rigidity frozen
Lösung
1) Reduce cooling rate to make crystallization complete and reduce hard feel; 2) reduce filler addition amount; 3) add plasticizer 0.5wt% to reduce hardness
Wichtigste Erkenntnis
High hardness is caused by crystallization and filler; adjusting cooling and filler are key
DSTDPhardness too highcrystallinityfiller amountplasticizer