Material Analysis 8 visualizaciones

DSTDP hardness too high

Fenómeno del problema
DSTDP product Shore hardness 5-10 degrees higher than target, hard hand feel
Análisis de la causa
DSTDP crystallinity on the high side, rigidity increased; filler added too much; cooling too fast, crystallization incomplete but rigidity frozen
Solución
1) Reduce cooling rate to make crystallization complete and reduce hard feel; 2) reduce filler addition amount; 3) add plasticizer 0.5wt% to reduce hardness
Conclusión clave
High hardness is caused by crystallization and filler; adjusting cooling and filler are key
DSTDPhardness too highcrystallinityfiller amountplasticizer