Material Analysis
4 조회수
DSTDP hardness too high
문제 현상
DSTDP product Shore hardness 5-10 degrees higher than target, hard hand feel
원인 분석
DSTDP crystallinity on the high side, rigidity increased; filler added too much; cooling too fast, crystallization incomplete but rigidity frozen
해결 방법
1) Reduce cooling rate to make crystallization complete and reduce hard feel; 2) reduce filler addition amount; 3) add plasticizer 0.5wt% to reduce hardness
핵심 요약
High hardness is caused by crystallization and filler; adjusting cooling and filler are key