Material Analysis
5 görüntüleme
DSTDP hardness too high
Sorun Belirtisi
DSTDP product Shore hardness 5-10 degrees higher than target, hard hand feel
Neden Analizi
DSTDP crystallinity on the high side, rigidity increased; filler added too much; cooling too fast, crystallization incomplete but rigidity frozen
Çözüm
1) Reduce cooling rate to make crystallization complete and reduce hard feel; 2) reduce filler addition amount; 3) add plasticizer 0.5wt% to reduce hardness
Temel Çıkarım
High hardness is caused by crystallization and filler; adjusting cooling and filler are key
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu