Injection Molding 3 Aufrufe

PETG '2079851475616104452 machine nozzle freezing and clogging

Problembeschreibung
During PETG '2079851475616104452, the material at the nozzle freezes and clogs, making normal injection impossible.
Ursachenanalyse
Nozzle temperature low (below the melting temperature), contact between mold and nozzle causes excessive cooling, material cools during long shutdown.
Lösung
Increase the nozzle temperature to 240-250°C; reduce the contact area between the nozzle and the mold (insulation pad); manually purge before shutdown.
Wichtigste Erkenntnis
PETG nozzle freezing is a common problem of temperature control and thermal management.