Menu
Materials Machinery
Insights
Articles Videos Problem & Solution
About
About Chembull Media Partners
Contact Us
Language
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
Back to Problem & Solution
Injection Molding 2 views

PETG '2079851475616104452 machine nozzle freezing and clogging

Problem Phenomenon
During PETG '2079851475616104452, the material at the nozzle freezes and clogs, making normal injection impossible.
Cause Analysis
Nozzle temperature low (below the melting temperature), contact between mold and nozzle causes excessive cooling, material cools during long shutdown.
Solution
Increase the nozzle temperature to 240-250°C; reduce the contact area between the nozzle and the mold (insulation pad); manually purge before shutdown.
Key Takeaway
PETG nozzle freezing is a common problem of temperature control and thermal management.
PETGnozzle freezingcloggingnozzle temperatureheat insulation

Was this helpful?

0 people found this helpful