Injection Molding 7 visualizações

PETG '2079851475616104452 machine nozzle freezing and clogging

Fenómeno do problema
During PETG '2079851475616104452, the material at the nozzle freezes and clogs, making normal injection impossible.
Análise das causas
Nozzle temperature low (below the melting temperature), contact between mold and nozzle causes excessive cooling, material cools during long shutdown.
Solução
Increase the nozzle temperature to 240-250°C; reduce the contact area between the nozzle and the mold (insulation pad); manually purge before shutdown.
Conclusão principal
PETG nozzle freezing is a common problem of temperature control and thermal management.
PETGnozzle freezingcloggingnozzle temperatureheat insulation

Isto foi útil?

0 pessoas acharam isto útil

ChemAI