Injection Molding 8 visualizaciones

PETG '2079851475616104452 machine nozzle freezing and clogging

Fenómeno del problema
During PETG '2079851475616104452, the material at the nozzle freezes and clogs, making normal injection impossible.
Análisis de la causa
Nozzle temperature low (below the melting temperature), contact between mold and nozzle causes excessive cooling, material cools during long shutdown.
Solución
Increase the nozzle temperature to 240-250°C; reduce the contact area between the nozzle and the mold (insulation pad); manually purge before shutdown.
Conclusión clave
PETG nozzle freezing is a common problem of temperature control and thermal management.
PETGnozzle freezingcloggingnozzle temperatureheat insulation

¿Le ha resultado útil?

0 personas encontraron esto útil