Material Drying 3 Aufrufe

PAEK product bubbles/internal pores

Problembeschreibung
Internal bubbles appear in PAEK injection molded products, affecting mechanical properties
Ursachenanalyse
Insufficient drying, moisture content exceeding the standard (PAEK requires 150-180°C/2-3h drying); at processing temperatures of 350-400°C, trace moisture vaporizes sharply
Lösung
Strictly dry to moisture content <0.02%; reduce screw speed; increase holding pressure time and pressure
Wichtigste Erkenntnis
PAEK is similar to PEEK in that trace moisture causes bubbles at extremely high processing temperatures