Q
PP Part Surface Ripple (Flow Mark)
A
Ripple = disordered front rhythm—smooth out the speed profile.
Molds & Tooling PP;ripple;melt front;speed profile;mold temperature
Q
PP Glass Fiber Reinforced Warpage
A
Orientation warpage is broken through from gate design.
Molds & Tooling PP;glass fiber;warpage;orientation;gate
Q
PP Mold Sticking
A
For mold sticking, reduce pressure first, then fix draft and polishing.
Molds & Tooling PP;mold sticking;holding pressure;draft angle;polishing
Q
PP Jetting Mark
A
Hit the wall first then spread—jetting marks come no more.
Molds & Tooling PP;jetting mark;gate;injection speed;snake-like mark
Q
PP Weak Weld Line Strength
A
PP weld lines must complete entanglement before crystallization.
Molds & Tooling PP;weld line;crystallization;venting;melt temperature
Q
PP Dimensional Post-shrinkage Drift
A
PP dimensions should be managed by 'post-aging dimension'.
Molds & Tooling PP;post-shrinkage;post-crystallization;dimensional drift;annealing