HDPE '2079851475616104457 cycle too long
Fenómeno del problema
The '2079851475616104457 cycle is slow and capacity is limited.
Análisis de la causa
High melt temperature, high mold temperature, large wall thickness, and insufficient blowing pressure all prolong cooling and sizing time.
Solución
①Lower the melt temperature and mold temperature; ②optimize the wall thickness; ③increase the blowing pressure; ④adopt a refrigerated blowing air system.
Conclusión clave
Compress the cycle from both ends: temperature and blowing efficiency.
¿Le ha resultado útil?
0 personas encontraron esto útil