Blow Molding
12 görüntüleme
HDPE '2079851475616104457 cycle too long
Sorun Belirtisi
The '2079851475616104457 cycle is slow and capacity is limited.
Neden Analizi
High melt temperature, high mold temperature, large wall thickness, and insufficient blowing pressure all prolong cooling and sizing time.
Çözüm
①Lower the melt temperature and mold temperature; ②optimize the wall thickness; ③increase the blowing pressure; ④adopt a refrigerated blowing air system.
Temel Çıkarım
Compress the cycle from both ends: temperature and blowing efficiency.
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu
Geri bildiriminiz için teşekkürler!