Blow Molding
14 visualizações
HDPE '2079851475616104457 cycle too long
Fenómeno do problema
The '2079851475616104457 cycle is slow and capacity is limited.
Análise das causas
High melt temperature, high mold temperature, large wall thickness, and insufficient blowing pressure all prolong cooling and sizing time.
Solução
①Lower the melt temperature and mold temperature; ②optimize the wall thickness; ③increase the blowing pressure; ④adopt a refrigerated blowing air system.
Conclusão principal
Compress the cycle from both ends: temperature and blowing efficiency.