Extrusion & Post 10 visualizaciones

Insufficient strength of PP woven bag flat filaments

Fenómeno del problema
Flat filaments break frequently in the drawing process, and the tensile strength of finished woven bags does not meet the standard.
Análisis de la causa
Insufficient draw ratio makes the molecular orientation inadequate; the drawing temperature deviating from the optimal range also makes the strength build-up insufficient.; during on-site investigation, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience
Solución
①Optimize the draw ratio to the process upper limit; ②control the drawing temperature; ③check the melt index matching of the raw material; ④test the linear density uniformity of the flat filaments.; after adjustment, continuously sample and verify the effect, and resume mass production after confirming stability
Conclusión clave
Flat filament strength is built by drawing orientation; drawing process parameters are the core variables of drawing quality.; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
PP; flat filament; drawing; draw; strength; woven bag