Thermoforming 8 visualizaciones

PVC '2079851475616104458 Chill Marks

Fenómeno del problema
Cold lines and haze marks on product surface, corresponding to plug/mold surface contact areas.
Análisis de la causa
Hot sheet contacts cold plug/mold surface prematurely and is quenched; mold temperature too low; set before stretching is completed, leaving stress marks; during on-site troubleshooting, verify item by item according to this mechanism, avoid blindly adjusting the machine based solely on experience.
Solución
①Heat the plug; ②Appropriately increase mold temperature to improve melt replication and fit to cavity surface; ③Slow down plug speed; ④Balance heating zones; ⑤Check direct airflow blowing.
Conclusión clave
PVC chill mark = 'touching cold surface prematurely': raising mold temperature and slowing contact can eliminate it; a typical temperature management problem, unrelated to the material itself; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.
PVC; '2079851475616104458; chill mark; plug; mold temperature

¿Le ha resultado útil?

0 personas encontraron esto útil