Material Drying 8 visualizaciones

Silver streaks caused by moisture in EEA processing

Fenómeno del problema
White silver streaks appearing on the EEA injection molded product surface
Análisis de la causa
Raw material contains moisture >0.05% vaporizing during high-temperature processing forming bubbles stretched into silver streaks; insufficient drying or water vapor condensation in the hopper
Solución
1) Dry the raw material at 80°C for 3-4h to moisture <0.02%; 2) Increase back pressure 0.5-1MPa for venting; 3) Reduce injection speed to avoid air entrapment; 4) Heat the hopper to prevent water vapor condensation
Conclusión clave
Silver streaks are caused by moisture vaporization and stretching; drying and venting are the main countermeasures