Material Analysis
15 visualizaciones
EEA Strong Processing Odor
Fenómeno del problema
Obvious pungent odor in the EEA processing workshop
Análisis de la causa
EEA releases odorous volatiles at processing temperature (such as acetic acid, formaldehyde, etc.); additives decompose and release odor
Solución
1) Control processing temperature within the EEA recommended range to reduce decomposition; 2) Strengthen workshop ventilation and exhaust; 3) Add absorbent to neutralize odor
Conclusión clave
Strong odor is caused by EEA decomposition and volatilization; temperature control and ventilation are key
¿Le ha resultado útil?
0 personas encontraron esto útil
¡Gracias por sus comentarios!