Poor EMA antistatic effect

Fenómeno del problema
EMA product surface resistance >10¹²Ω with severe static electricity
Análisis de la causa
Antistatic agent addition insufficient <0.1wt%; antistatic agent migration rate slow, not reaching the surface
Solución
1) Increase antistatic agent to 0.3-0.5wt%; 2) Select antistatic agent with fast migration rate; 3) Surface coating with antistatic liquid for immediate effect
Conclusión clave
Poor antistatic effect is caused by insufficient addition; increasing antistatic agent is key
EMA antistatic antistatic agent surface resistance migration rate