EVA internal stress concentration is severe
Fenómeno del problema
EVA product internal stress >15MPa causes cracking during storage
Análisis de la causa
Injection speed too fast with large orientation stress; uneven cooling freezing thermal stress; improper gate position with concentrated flow orientation
Solución
1) Reduce injection speed to decrease orientation; 2) Uniform mold temperature to reduce thermal stress; 3) Annealing at 80°C/4h to release stress; 4) Optimize gate position
Conclusión clave
Internal stress is caused by fast injection and uneven cooling; reducing speed, uniform cooling, and annealing are key