Injection Molding
2 visualizaciones
Severe Internal Stress Concentration in EVOH
Fenómeno del problema
EVOH product internal stress >15MPa causing cracking during storage
Análisis de la causa
Injection speed too fast, orientation stress large; uneven cooling freezing thermal stress; gate location improper, flow orientation concentrated
Solución
1) Reduce injection speed to decrease orientation; 2) Uniform mold temperature to reduce thermal stress; 3) Anneal at 80°C/4h to release stress; 4) Optimize gate location
Conclusión clave
Internal stress is caused by fast injection and uneven cooling; speed reduction, uniform cooling and annealing are key