Injection Molding 1 visualizações

Severe Internal Stress Concentration in EVOH

Fenómeno do problema
EVOH product internal stress >15MPa causing cracking during storage
Análise das causas
Injection speed too fast, orientation stress large; uneven cooling freezing thermal stress; gate location improper, flow orientation concentrated
Solução
1) Reduce injection speed to decrease orientation; 2) Uniform mold temperature to reduce thermal stress; 3) Anneal at 80°C/4h to release stress; 4) Optimize gate location
Conclusão principal
Internal stress is caused by fast injection and uneven cooling; speed reduction, uniform cooling and annealing are key
EVOHinternal stressorientation stressannealinguniform cooling

Isto foi útil?