Bubbles in PU elastomer casting

Fenómeno del problema
Internal bubbles of 0.5-2mm in PU elastomer cast products
Análisis de la causa
Insufficient mixing and degassing; casting temperature too low, viscosity high, bubbles difficult to discharge
Solución
1) Vacuum degassing for 5-10min after mixing; 2) Increase casting temperature to 60-80°C to reduce viscosity and discharge bubbles; 3) Cast slowly to avoid air entrapment
Conclusión clave
PU casting bubbles are caused by insufficient degassing; vacuum degassing is key
PU casting bubbles vacuum degassing casting temperature mixing degassing