Molds & Tooling 8 visualizaciones

Cold slug marks appear on the product surface

Fenómeno del problema
Cold slug marks appear on the product surface, local poor gloss or hard lumps, usually near the gate
Análisis de la causa
Nozzle temperature too low, producing cold slug Front zone barrel temperature set low Mold sprue or runner temperature low, cold slug retained Mold opening gap too large, cold slug pulled into the cavity Screw pullback distance too large, producing cold slug
Solución
Increase nozzle temperature to prevent cold slug Appropriately increase the front zone barrel temperature Increase sprue and runner dimensions to reduce cold slug retention Reduce the mold opening gap Adjust the screw pullback distance
Conclusión clave
Cold slug marks require increasing nozzle temperature and reducing cold slug sources
cold slug marknozzle temperaturecold slug