Menú
Materiales Maquinaria
Perspectivas
Artículos Vídeos Problema y solución
About
Acerca de Chembull Socios de medios
Contáctenos
Idioma
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
Volver a Problema y solución
Extrusion & Post 14 visualizaciones

Glass Fibre extruder screw severe wear

Fenómeno del problema
After Glass Fibre extrusion 200h, screw and barrel wear reaches 0.5mm
Análisis de la causa
Filler causes large screw wear; screw material hardness insufficient, not nitrided; processing temperature too high causes Glass Fibre adhering to screw, aggravating wear
Solución
1) Use nitrided screw or bimetallic screw SK-2 alloy; 2) reduce processing temperature to reduce adhesive wear; 3) treat filler with coupling agent to reduce friction; 4) regularly check wear, replace in time when >0.3mm
Conclusión clave
Screw wear is caused by filler friction and adhesion; wear-resistant screw and temperature control are key
Glass Fibre extrusionscrew wearnitrided screwfiller frictionbimetallic screw

¿Le ha resultado útil?

0 personas encontraron esto útil

ChemAI