Extrusion & Post 14 visualizaciones

MP extruded profile bending deformation

Fenómeno del problema
MP extruded profiles continuously bend after cooling, bending deviation >5mm/m
Análisis de la causa
uneven cooling on each surface of the profile causes shrinkage difference; uneven die exit flow velocity makes profile wall thicknesses different; haul-off and extrusion centerlines misaligned producing lateral force
Solución
1) optimize the cooling system to ensure uniform cooling on all surfaces; 2) adjust the die so each wall has uniform flow velocity and consistent wall thickness; 3) align haul-off and extrusion centerlines; 4) increase calibrating sleeve length, cool after full calibration
Conclusión clave
profile bending is caused by uneven cooling and uneven flow velocity; homogenization and alignment are the keys to solving
MP extrusion bending deformation uniform cooling uniform flow velocity calibrating sleeve