MP large processing odor

Fenómeno del problema
MP processing workshop has an obvious pungent odor
Análisis de la causa
MP releases odorous volatiles (such as acetic acid, formaldehyde, etc.) at processing temperature; additives decompose releasing odor
Solución
1) control processing temperature within the MP recommended range to reduce decomposition; 2) strengthen workshop ventilation; 3) add absorbent to neutralize the odor
Conclusión clave
large odor is caused by MP decomposition volatilization; temperature control and ventilation are key
MP processing odor volatiles ventilation temperature control