Molding Process
9 visualizaciones
Yellowing of PMMA products
Fenómeno del problema
PMMA transparent products yellow and transparency decreases.
Análisis de la causa
Processing temperature too high >260°C or residence time too long causes thermal degradation; PMMA depolymerizes to produce monomer MMA which is colored.
Solución
Strictly control processing temperature at 200-240°C not exceeding 260°C; shorten residence time; use stabilized PMMA grades.
Conclusión clave
PMMA thermal stability is limited; strict temperature control is the key.
¿Le ha resultado útil?
0 personas encontraron esto útil