Injection Molding
8 visualizaciones
Flash and burrs on products
Fenómeno del problema
Thin sheet-like excess material appears at the mold parting line, affecting assembly
Análisis de la causa
Clamping force is insufficient to resist cavity pressure; injection pressure peak is too high, causing the mold to open; the mold parting line is worn or has foreign matter
Solución
Verify clamping force ≥ cavity projected area × (40-80MPa); reduce injection/holding peak pressure; check and repair the mold parting line
Conclusión clave
Flash reflects the matching problem between the clamping system and injection pressure
¿Le ha resultado útil?
0 personas encontraron esto útil