Injection Molding
4 조회수
HDPE '2079851475616104452 sink marks
문제 현상
Depressions at thick-walled areas and behind ribs.
원인 분석
High shrinkage + insufficient holding pressure compensation; the gate freezes too early.
해결 방법
①Increase holding pressure and time; ②enlarge the gate; ③rib thickness ≤60% of wall thickness; ④reduce material in thick walls.
핵심 요약
Sink marks are tackled with both holding pressure and structural material reduction.
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!