Injection Molding 5 görüntüleme

HDPE '2079851475616104452 sink marks

Sorun Belirtisi
Depressions at thick-walled areas and behind ribs.
Neden Analizi
High shrinkage + insufficient holding pressure compensation; the gate freezes too early.
Çözüm
①Increase holding pressure and time; ②enlarge the gate; ③rib thickness ≤60% of wall thickness; ④reduce material in thick walls.
Temel Çıkarım
Sink marks are tackled with both holding pressure and structural material reduction.