Molds & Tooling 4 조회수

CEF internal shrinkage cavity

문제 현상
Shrinkage cavities with a diameter of 0.5-2mm appear in the center of the CEF thick-walled product
원인 분석
The thick-walled area shrinks internally after cooling but the surface has solidified and cannot be fed; the holding pressure time is insufficient and the gate freezes too early
해결 방법
1) Extend the holding pressure time until the gate is completely frozen; 2) Increase the gate size to delay freezing; 3) Product design to reduce wall thickness differences
핵심 요약
Shrinkage cavities are caused by thick wall shrinkage and insufficient holding pressure; extending the holding pressure is the key