Molds & Tooling
7 visualizações
CEF internal shrinkage cavity
Fenómeno do problema
Shrinkage cavities with a diameter of 0.5-2mm appear in the center of the CEF thick-walled product
Análise das causas
The thick-walled area shrinks internally after cooling but the surface has solidified and cannot be fed; the holding pressure time is insufficient and the gate freezes too early
Solução
1) Extend the holding pressure time until the gate is completely frozen; 2) Increase the gate size to delay freezing; 3) Product design to reduce wall thickness differences
Conclusão principal
Shrinkage cavities are caused by thick wall shrinkage and insufficient holding pressure; extending the holding pressure is the key