Extrusion & Post
10 조회수
DSTDP extrusion rough surface
문제 현상
DSTDP extruded product surface roughness Ra>5μm, exceeding requirements
원인 분석
Extrusion temperature on the low side <160°C, melt flow unstable; die inner wall rough or damaged; DSTDP melt elasticity, extrusion swell uneven
해결 방법
1) Raise extrusion temperature to 160-200°C; 2) polish die inner wall Ra<0.4μm; 3) reduce extrusion rate 10-15%; 4) add 0.3-0.5wt% external lubricant
핵심 요약
Rough surface is caused by low-temperature extrusion and die defects; raising temperature and polishing the die are the core countermeasures