Extrusion & Post
11 görüntüleme
DSTDP extrusion rough surface
Sorun Belirtisi
DSTDP extruded product surface roughness Ra>5μm, exceeding requirements
Neden Analizi
Extrusion temperature on the low side <160°C, melt flow unstable; die inner wall rough or damaged; DSTDP melt elasticity, extrusion swell uneven
Çözüm
1) Raise extrusion temperature to 160-200°C; 2) polish die inner wall Ra<0.4μm; 3) reduce extrusion rate 10-15%; 4) add 0.3-0.5wt% external lubricant
Temel Çıkarım
Rough surface is caused by low-temperature extrusion and die defects; raising temperature and polishing the die are the core countermeasures
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu
Geri bildiriminiz için teşekkürler!