Injection Molding
3 조회수
MP Periodic Surface Ripples
문제 현상
Periodic ripples with 5-15mm spacing on the surface of MP products
원인 분석
Periodic fluctuation of injection speed; unstable hydraulic system; unstable screw rotation speed
해결 방법
1) Overhaul the injection system to stabilize pressure and speed; 2) Replace hydraulic drive with servo motor drive; 3) PID control to stabilize injection parameters
핵심 요약
Ripples are caused by unstable injection; equipment overhaul and PID control are key
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다