Injection Molding 4 views

PA6 Short Shot

Problem Phenomenon
Material shortage at the ends of thin-wall parts and long-flow parts.
Cause Analysis
PA6 solidifies quickly, and the flow front freezes quickly at thin walls; insufficient injection speed/pressure and low mold temperature.
Solution
①Increase injection speed and pressure;②increase material temperature and mold temperature;③enlarge the gate;④select high-flow grades for thin-wall parts.
Key Takeaway
PA6 short shot = a race against freezing speed.
PA6; short shot; fast solidification; injection speed; mold temperature