Molding Process 5 views

CPE Melting and Plasticization Difficulty

Problem Phenomenon
CPE plasticizes slowly at processing temperature
Cause Analysis
CPE is amorphous but has hydrogen-bond physical crosslinking
Solution
Raise processing temperature and increase shear
Key Takeaway
CPE plasticization requires sufficient shear and temperature