Molding Process 5 views

Internal shrinkage porosity in thick-walled PVC products

Problem Phenomenon
Loose or voids in the center of thick-walled parts
Cause Analysis
Center cools slowly, feeding flow channel solidifies too early
Solution
Optimize gate position and size, extend holding pressure, increase pressure
Key Takeaway
Internal quality of thick-walled parts is a technical difficulty