Injection Molding 1 views

EMA surface tiger stripes

Problem Phenomenon
Tiger stripe alternating light and dark bands 2-5mm wide on EMA injection molded product surface
Cause Analysis
Unstable injection speed with melt front fluctuating fast and slow; mold temperature too low <30°C causing rapid front cooling
Solution
1) Multi-stage injection slow-fast-slow to stabilize the front; 2) Increase mold temperature to 40-50°C; 3) Increase injection pressure for stable advancement
Key Takeaway
Tiger stripes are caused by unstable injection front; multi-stage injection and high mold temperature are key
EMA tiger stripes injection speed multi-stage injection mold temperature control