Menu
Materials Machinery
Insights
Articles Videos Problem & Solution
About
About Chembull Media Partners
Contact Us
Language
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
Back to Problem & Solution
Extrusion & Post 8 views

Gel Particles in CMC Extruded Film

Problem Phenomenon
Transparent gel particles of 0.1-0.5mm appear on the surface of CMC extruded film
Cause Analysis
High-molecular-weight components in CMC are not fully melted during extrusion, forming local high-crystallinity zones; extrusion temperature is low or mixing is insufficient
Solution
1)Increase extrusion temperature by 5-10°C to ensure full melting; 2)Increase screw mixing section length; 3)Inspect raw materials to ensure consistent grade; 4)Replace with finer 120-mesh screen to intercept unmelted particles
Key Takeaway
Gel particles are caused by insufficient melting; increasing temperature and mixing are the key
CMC filmgel particlesmelting temperaturemixing sectionhigh-molecular-weight components

Was this helpful?

0 people found this helpful

ChemAI