MP '2079851475616104452 flow marks

Problem Phenomenon
MP injection molded product surface shows radial flow marks centered on the gate
Cause Analysis
injection speed too fast causing unstable melt front; mold temperature too low <30°C, front rapidly cools forming marks
Solution
1) adopt multi-stage injection speed slow-fast-slow to control front stability; 2) raise mold temperature to 40-50°C to delay front cooling; 3) stabilize injection pressure to avoid fluctuation; 4) enlarge gate area to reduce pressure sudden change at the gate
Key Takeaway
flow marks are caused by unstable injection front and rapid cooling; multi-stage injection and high mold temperature are key
MP injection flow mark injection speed mold temperature gate area