Molding Process 5 views

PBN surface roughness problem in sheet processing

Problem Phenomenon
Polybutylene naphthalate PBN shows surface roughness in sheet processing at 270-300°C.
Cause Analysis
Degradation under high-temperature processing at 270-300°C triggers the problem.
Solution
Solved by precise temperature control.
Key Takeaway
PBN ultra-high-temperature processing requires comprehensive protection.
PBNsurface roughnesshigh temperaturesheetprotection